1. Mainly for thermoplastic methacrylate resin with calcium carbonate, pigment powder, talcum powder, xylene, etc.
2. Quick drying, strong adhesion and easy construction. Use by a certain proportion of xylene or day that water mixing can be constructed.
3. Poor heat resistance and solvent resistance. When the heating temperature exceeds 177-232℃, degradation into monomer will occur from solubility to adhesion in the case of strong solvent after curing.